Citation: | GU Chao, ZHAO Li-hua, GAN Peng. Revolution and control of Fe-Al-Ti-O complex oxide inclusions in ultralow-carbon steel during refining process[J]. Chinese Journal of Engineering, 2019, 41(6): 757-762. doi: 10.13374/j.issn2095-9389.2019.06.007 |
[1] |
Wang R, Bao Y P, Li Y H, et al. Effect of slag composition on steel cleanliness in interstitial-free steel. J Iron Steel Res Int, 2017, 24(6): 579 doi: 10.1016/S1006-706X(17)30088-2
|
[2] |
Deng X X, Ji C X, Guan S K, et al. Inclusion behaviour in aluminium-killed steel during continuous casting. Ironmaking Steelmaking, 2018: 1 doi: 10.1080/03019233.2018.1428420
|
[3] |
Yu H X, Ji C X, Chen B, et al. Characteristics and evolution of inclusion induced surface defects of cold rolled IF sheet. J Iron Steel Res Int, 2015, 22(Suppl1): 17
|
[4] |
趙子蘇, 毛衛民, 余永寧, 等. 鈦對高強IF鋼第二相粒子析出規律和力學性能的影響. 鋼鐵, 2000, 35(9): 47 doi: 10.3321/j.issn:0449-749X.2000.09.014
Zhao Z S, Mao W M, Yu Y N, et al. Effect of Ti on precipitation of second phase particals and mechanical properties of high strength IF steel. Iron Steel, 2000, 35(9): 47 doi: 10.3321/j.issn:0449-749X.2000.09.014
|
[5] |
Wang M, Bao Y P, Cui H, et al. The composition and morphology evolution of oxide inclusions in Ti-bearing ultra low-carbon steel melt refined in the RH process. ISIJ Int, 2010, 50(11): 1606 doi: 10.2355/isijinternational.50.1606
|
[6] |
隋亞飛, 孫國棟, 趙艷, 等. IF鋼中含Ti夾雜物的衍變規律. 北京科技大學學報, 2014, 36(9): 1174 https://www.cnki.com.cn/Article/CJFDTOTAL-BJKD201409007.htm
Sui Y F, Sun G D, Zhao Y, et al. Evolution of titaniferous inclusions in IF steelmaking. J Univ Sci Technol Beijing, 2014, 36(9): 1174 https://www.cnki.com.cn/Article/CJFDTOTAL-BJKD201409007.htm
|
[7] |
Qin Y M, Wang X H, Huang F X, et al. Influence of reoxidation by slag and air on inclusions in IF steel. Metall Res Technol, 2015, 112(4): 405 doi: 10.1051/metal/2015025
|
[8] |
Tsunekawa H, Yamashita T, Aoyama T, et al. Mechanism of formation of streak-shaped defects on ultra-low carbon IF steel for automobile outer panels after press forming and influence of slab reheating temperature before hot rolling and Sb-addition on defects. Tetsu-to-Hagane, 2016, 102(4): 202 doi: 10.2355/tetsutohagane.TETSU-2015-061
|
[9] |
Gutiérrez E, Garcia-Hernandez S, de Jesús Barreto J. Mathematical analysis of the dynamic effects on the deposition of alumina inclusions inside the upper tundish nozzle. ISIJ Int, 2016, 56(8): 1394 doi: 10.2355/isijinternational.ISIJINT-2016-076
|
[10] |
Guo J L, Bao Y P, Wang M. Cleanliness of Ti-bearing Al-killed ultra-low-carbon steel during different heating processes. Int J Miner Metall Mater, 2017, 24(12): 1370 doi: 10.1007/s12613-017-1529-8
|
[11] |
Chase Jr M W, Curnutt J L, McDonald R A, et al. JANAF thermochemical tables, 1978 supplement. J Phys Chem Ref Data, 1978, 7(3): 793 doi: 10.1063/1.555580
|
[12] |
Kubaschewski O, Dench W A. The free-energy diagram of the system titanium-oxygen. J Inst Met, 1953: 82 http://ci.nii.ac.jp/naid/10009581664
|
[13] |
Nakajima K. Estimation of interfacial tensions between phases in the molten iron-slag-inclusion (alumina) system. Tetsu-toHagane, 1994, 80(5): 383 doi: 10.2355/tetsutohagane1955.80.5_383
|
[14] |
Zhao L Y, Sahajwalla V. Interfacial phenomena during wetting of graphite/alumina mixtures by liquid iron. ISIJ Int, 2003, 43(1): 1 doi: 10.2355/isijinternational.43.1
|
[15] |
Yang G W, Wang X H, Huang F X, et al. Transient Inclusion Evolution during RH Degassing. Steel Res Int, 2014, 85(1): 26 doi: 10.1002/srin.201300030
|
[16] |
Xuan C J, Shibata H, Sukenaga S, et al. Wettability of Al2O3, MgO and Ti2O3 by liquid iron and steel. ISIJ Int, 2015, 55(9): 1882 doi: 10.2355/isijinternational.ISIJINT-2014-820
|
[17] |
Yang G W, Wang X H, Huang F X, et al. Transient inclusion evolution during RH degassing. Steel Res Int, 2014, 85(1): 26 doi: 10.1002/srin.201300030
|