<listing id="l9bhj"><var id="l9bhj"></var></listing>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<var id="l9bhj"></var><cite id="l9bhj"><video id="l9bhj"></video></cite>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"><listing id="l9bhj"></listing></strike></cite><cite id="l9bhj"><span id="l9bhj"><menuitem id="l9bhj"></menuitem></span></cite>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<ins id="l9bhj"><span id="l9bhj"></span></ins>
Volume 30 Issue 7
Aug.  2021
Turn off MathJax
Article Contents
CAI Yuanhua, JI Fei, WANG Mingji, HUANG Jinfeng, DUAN Xianjin, ZHANG Jishan. Microstructure and properties of spray-formed high-strength Al-Zn-Mg-Cu alloy containing manganese[J]. Chinese Journal of Engineering, 2008, 30(7): 756-759,774. doi: 10.13374/j.issn1001-053x.2008.07.036
Citation: CAI Yuanhua, JI Fei, WANG Mingji, HUANG Jinfeng, DUAN Xianjin, ZHANG Jishan. Microstructure and properties of spray-formed high-strength Al-Zn-Mg-Cu alloy containing manganese[J]. Chinese Journal of Engineering, 2008, 30(7): 756-759,774. doi: 10.13374/j.issn1001-053x.2008.07.036

Microstructure and properties of spray-formed high-strength Al-Zn-Mg-Cu alloy containing manganese

doi: 10.13374/j.issn1001-053x.2008.07.036
  • Received Date: 2007-04-23
  • Rev Recd Date: 2007-10-16
  • Available Online: 2021-08-06
  • An Al-Zn-Mg-Cu alloy containing 2% Mn (mass fraction) was prepared by spray forming method and hot extrusion. The microstructure and mechanical properties of the spray-deposited Al alloy were studied by optical microscopy, scanning electron microscopy, X-ray diffraction, and tensile tests. The results show that the Al alloy has uniformly fine recrystallized grains with an average size of 8μm after hot extrusion and solid solution treatment. MnAl6 particles were precipitated at grain boundaries during the spray forming process, most of the MnAl6 particles were plastically deformed to some extent along the direction of extrusion during the hot extrusion process, and some large MnAl6 particles were fragged. The effect of solution treatment on the size of MnAl6 particles is negligible but the spheroidization of rod-like/plate-like particles occurred at the corner of these particles. The spheroidization of MnAl6 particles is benefit to the decrease of stress or strain concentration which would induce microcracks. When aged at 120℃ for 24 h, the tensile strength of the Al alloy was increased up to 775 MPa with an elongation of 4.3%, and the fracture surface consisted mainly of dimples with a size lower than 500 nm.

     

  • loading
  • 加載中

Catalog

    通訊作者: 陳斌, bchen63@163.com
    • 1. 

      沈陽化工大學材料科學與工程學院 沈陽 110142