<listing id="l9bhj"><var id="l9bhj"></var></listing>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<var id="l9bhj"></var><cite id="l9bhj"><video id="l9bhj"></video></cite>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"><listing id="l9bhj"></listing></strike></cite><cite id="l9bhj"><span id="l9bhj"><menuitem id="l9bhj"></menuitem></span></cite>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<ins id="l9bhj"><span id="l9bhj"></span></ins>
Volume 30 Issue 3
Aug.  2021
Turn off MathJax
Article Contents
LU Xin, HE Xinbo, LI Shiqiong, QU Xuanhui. Microstructures and mechanical properties of TiAl-based alloys by spark plasma sintering[J]. Chinese Journal of Engineering, 2008, 30(3): 254-257. doi: 10.13374/j.issn1001-053x.2008.03.010
Citation: LU Xin, HE Xinbo, LI Shiqiong, QU Xuanhui. Microstructures and mechanical properties of TiAl-based alloys by spark plasma sintering[J]. Chinese Journal of Engineering, 2008, 30(3): 254-257. doi: 10.13374/j.issn1001-053x.2008.03.010

Microstructures and mechanical properties of TiAl-based alloys by spark plasma sintering

doi: 10.13374/j.issn1001-053x.2008.03.010
  • Received Date: 2006-12-08
  • Rev Recd Date: 2007-01-14
  • Available Online: 2021-08-06
  • TiAl based alloys from the prealloyed powder of Ti-47.5Al-2.5V-1.0Cr were prepared by spark plasma sintering (SPS), and the relationship among sintering temperature, microstructure and mechanical properties was studied. The results showed that the TiAl based-alloy with high density and uniform microstructure could be obtained by SPS. In addition, the microstructure changed with sintering temperature, as a result, the mechanical properties changed with the microstructure. The finer the microstructure was, the higher the strength and ductility at room temperature became. For specimens sintered at 1100℃, the finer duplex microstructure was achieved. The specimens exhibited better compressive properties at room temperature with a compressive strength of 3 321 MPa and a compression ratio of 35.2%.

     

  • loading
  • 加載中

Catalog

    通訊作者: 陳斌, bchen63@163.com
    • 1. 

      沈陽化工大學材料科學與工程學院 沈陽 110142

    1. 本站搜索
    2. 百度學術搜索
    3. 萬方數據庫搜索
    4. CNKI搜索
    Article views (175) PDF downloads(5) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return
    久色视频