Citation: | HAO Yang, BAO Yan-ping, LI Ren-chun, LI Tai-quan, CHENG Di, CHEN Xiao, WANG Rui. Influence of key parameters in steelmaking progress on the inclusion defects of rolled IF steel sheet[J]. Chinese Journal of Engineering, 2017, 39(3): 369-376. doi: 10.13374/j.issn2095-9389.2017.03.008 |
[2] |
Cui H, Wu H J, Yue F, et al. Surface defects of cold-rolled Ti-IF steel sheets due to non-metallic inclusions. J Iron Steel Res Int, 2011, 18(Suppl 2):335
|
[9] |
Miyake T, Morishita M, Nakata H, et al. Influence of sulphur content and molten steel flow on entrapment of bubbles to solid/liquid interface. ISIJ Int, 2006, 46(12):1817
|
[10] |
Yu H X, Ji C X, Chen B, et al. Characteristics and evolution of inclusion induced surface defects of cold rolled IF sheet. J Iron Steel Res Int, 2015, 22(Suppl 1):17
|
[11] |
Chen Y, Zeng J H, Wu G R. Control for surface faint-sliver defects in cold-rolled IF steel sheet. Adv Mater Res, 2011, 396-398:1145
|