<listing id="l9bhj"><var id="l9bhj"></var></listing>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<var id="l9bhj"></var><cite id="l9bhj"><video id="l9bhj"></video></cite>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"><listing id="l9bhj"></listing></strike></cite><cite id="l9bhj"><span id="l9bhj"><menuitem id="l9bhj"></menuitem></span></cite>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<ins id="l9bhj"><span id="l9bhj"></span></ins>
Volume 35 Issue 6
Jul.  2021
Turn off MathJax
Article Contents
LIN Lu, BAO Yan-ping, WANG Min, ZHOU Han-mei, ZHANG Li-qiang. Phosphorus behavior in CaO-SiO2-FeO slag during converter melting process[J]. Chinese Journal of Engineering, 2013, 35(6): 720-724. doi: 10.13374/j.issn1001-053x.2013.06.015
Citation: LIN Lu, BAO Yan-ping, WANG Min, ZHOU Han-mei, ZHANG Li-qiang. Phosphorus behavior in CaO-SiO2-FeO slag during converter melting process[J]. Chinese Journal of Engineering, 2013, 35(6): 720-724. doi: 10.13374/j.issn1001-053x.2013.06.015

Phosphorus behavior in CaO-SiO2-FeO slag during converter melting process

doi: 10.13374/j.issn1001-053x.2013.06.015
  • Received Date: 2012-03-01
  • An expression was regressed to describe the relation of phosphate capacity in slag to slag's optical basicity and temperature. An iso-phosphate capacity graph of the CaO-SiO2-FeO (10% MgO) slag system was depicted by the regression expression. The effect of converter end-point slag, end-point composition and temperature on the phosphorus content in steel was analyzed. When the phosphate capacity in slag is constant, the distribution ratio of phosphorus between slag and steel increases with the converter final carbon content decreasing; but at a constant final carbon content, with the increase of phosphate capacity in slag, the distribution ratio of phosphorus between slag and steel increases. It is suggested that the final carbon content is controlled between 0.03% and 0.04%, the slag basicity is more than 3.5, the FeO content in slag is less than 18%, and the P2O5 content in slag is less than 2%, which are favorable for producing liquid steel with the final phosphorus content less than 0.008%.

     

  • loading
  • 加載中

Catalog

    通訊作者: 陳斌, bchen63@163.com
    • 1. 

      沈陽化工大學材料科學與工程學院 沈陽 110142

    1. 本站搜索
    2. 百度學術搜索
    3. 萬方數據庫搜索
    4. CNKI搜索
    Article views (185) PDF downloads(9) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return
    久色视频