<listing id="l9bhj"><var id="l9bhj"></var></listing>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<var id="l9bhj"></var><cite id="l9bhj"><video id="l9bhj"></video></cite>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"><listing id="l9bhj"></listing></strike></cite><cite id="l9bhj"><span id="l9bhj"><menuitem id="l9bhj"></menuitem></span></cite>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<ins id="l9bhj"><span id="l9bhj"></span></ins>
Volume 32 Issue 5
Aug.  2021
Turn off MathJax
Article Contents
ZHU Guan-ni, BI Zhong-nan, DONG Jian-xin, ZHANG Mai-cang, ZHENG Lei, ZHANG Qing-quan. Microsegregation and homogenization of nickel base corrosion resistant alloy C-276 ingots[J]. Chinese Journal of Engineering, 2010, 32(5): 628-633,656. doi: 10.13374/j.issn1001-053x.2010.05.017
Citation: ZHU Guan-ni, BI Zhong-nan, DONG Jian-xin, ZHANG Mai-cang, ZHENG Lei, ZHANG Qing-quan. Microsegregation and homogenization of nickel base corrosion resistant alloy C-276 ingots[J]. Chinese Journal of Engineering, 2010, 32(5): 628-633,656. doi: 10.13374/j.issn1001-053x.2010.05.017

Microsegregation and homogenization of nickel base corrosion resistant alloy C-276 ingots

doi: 10.13374/j.issn1001-053x.2010.05.017
  • Received Date: 2009-09-22
  • The microstructure and microsegregation of nickel base corrosion resistant alloy C-276 vacuum-induction-melting and electroslag-remelting ingots were studied by optical microscope, scanning electron microscopy and energy dispersive X-ray spectroscopy. Based on the calculated results of the residual segregation parameter model, four homogenizing treatments were tested. Microstructure analysis and thermal compression test with a Gleeble 1500 machine were used to verify the effect of homogenizing treatment. The results show that the severest segregated elements in C-276 is Mo, and 1170℃/20h is the most appropriate treatment for C-276 alloy in the study as it ensures homogenizing effect and reasonable grain size for optimizing the hot-working plasticity of the alloy. It is also proved that homogenization process of C-276 alloy can be effectively predicted and evaluated by the residual segregation parameter model, which basically agrees with the experimental results.

     

  • loading
  • 加載中

Catalog

    通訊作者: 陳斌, bchen63@163.com
    • 1. 

      沈陽化工大學材料科學與工程學院 沈陽 110142