<listing id="l9bhj"><var id="l9bhj"></var></listing>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<cite id="l9bhj"><strike id="l9bhj"></strike></cite>
<var id="l9bhj"></var><cite id="l9bhj"><video id="l9bhj"></video></cite>
<menuitem id="l9bhj"></menuitem>
<cite id="l9bhj"><strike id="l9bhj"><listing id="l9bhj"></listing></strike></cite><cite id="l9bhj"><span id="l9bhj"><menuitem id="l9bhj"></menuitem></span></cite>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"></var>
<var id="l9bhj"><strike id="l9bhj"></strike></var>
<ins id="l9bhj"><span id="l9bhj"></span></ins>
Volume 27 Issue 5
Aug.  2021
Turn off MathJax
Article Contents
ZHAO Fang, LIN Tao, ZHANG Liying, WU Chengyi. Sintering and mechanical properties of nanoscaled W-40%Cu alloys[J]. Chinese Journal of Engineering, 2005, 27(5): 577-581. doi: 10.13374/j.issn1001-053x.2005.05.047
Citation: ZHAO Fang, LIN Tao, ZHANG Liying, WU Chengyi. Sintering and mechanical properties of nanoscaled W-40%Cu alloys[J]. Chinese Journal of Engineering, 2005, 27(5): 577-581. doi: 10.13374/j.issn1001-053x.2005.05.047

Sintering and mechanical properties of nanoscaled W-40%Cu alloys

doi: 10.13374/j.issn1001-053x.2005.05.047
  • Received Date: 2004-09-04
  • Rev Recd Date: 2005-03-15
  • Available Online: 2021-08-17
  • The densification of nanoscaled W-Cu powder was investigated through measurements of the shrinkage kinetic curves in hot pressing and hydrogen sintering and compared with that of nanoscaled W powder and traditional Cu powder. The resulted alloys were subjected to hot compression tests at 300℃ and 500℃ to obtain their stress-strain curves. It is indicated that the temperature corresponding to the highest shrinkage rate of nanoscaled W-Cu powder is 980℃ in hydrogen sintering. After sintering at 1200℃, the mean grain size of W phase is less than 2 μm, and the relative density of the alloy is 97%. In hot pressing, however the corresponding temperatures is 930℃. The mean grain size of W phase in the hot pressed alloy from nanoscaled W-Cu powder is 0.5μm at 1 200℃, and its relative density is 98%. The results of hot compression tests at 300℃ and 500℃ showed that the high-temperature strength of the ultrafine grained W-Cu alloy is higher than that of the alloy sintered from nanoscaled W powder and traditional Cu powder.

     

  • loading
  • 加載中

Catalog

    通訊作者: 陳斌, bchen63@163.com
    • 1. 

      沈陽化工大學材料科學與工程學院 沈陽 110142

    1. 本站搜索
    2. 百度學術搜索
    3. 萬方數據庫搜索
    4. CNKI搜索
    Article views (272) PDF downloads(7) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return
    久色视频