Effect of the hot charging temperature of slabs on A1N and MnS precipitation behavior in non-oriented silicon steel
-
摘要: 通過固溶度積公式計算及熱模擬實驗,對不同熱裝和加熱溫度條件下的無取向硅鋼鑄坯中析出相進行了研究.在低于950℃熱裝時,鑄坯中AlN的析出量和尺寸不再變化,但MnS和AlN-MnS的數量及平均尺寸隨著熱裝溫度降低而進一步增加,并在溫度低于600℃時達到最大值后保持不變.與1200℃相比,1100℃加熱的鑄坯中AlN、MnS的總固溶量相對更少.相比850℃熱裝,600℃熱裝再加熱到1100℃的鑄坯中AlN和MnS的總固溶量更少,且AlN和MnS尺寸更大.合適的熱裝溫度和加熱溫度分別為600℃和1100℃.Abstract: Based on solubility product calculation and thermal simulation experiments, precipitated phases in continuous casting slabs of non-oriented silicon steel were systematically studied at different hot charging and heating temperatures. When the hot charging temperature is below 950℃, the content and size of A1N remain unchanged, but the quantity and size of MnS and A1N-MnS increase when the hot charging temperature decreases, reach maximum and remain unchanged when the hot charging temperature is below 600℃. The total content of A1N and MnS solid solution in the slab heated at 1100℃ is less than that heated at 1200℃. Compared with the slab hot-charged at 850℃ and heated at 1100℃, the total content of A1N and MnS solid solution is less and the size of A1N and MnS is larger in the slab hot-charged at 600℃ and heated at 1100℃. The appropriate hot charging temperature and heating temperature are 600℃ and 1100℃, respectively.
-
Key words:
- silicon steel /
- temperature /
- precipitation /
- aluminum nitride /
- manganese sulfide
-

計量
- 文章訪問數: 176
- HTML全文瀏覽量: 33
- PDF下載量: 16
- 被引次數: 0