Whole-tailings backfilling materials with fly ash
-
摘要: 實驗選取了Ⅰ級和Ⅱ級兩種粉煤灰,以石灰和脫硫石膏為激發劑制備的膠凝材料完全取代傳統的膠結劑水泥,以膠砂比為1:4,水膠比為1:1左右制備的粉煤灰全尾砂充填料在45±1℃下養護3 d,強度可達5.432 MPa,在20±1℃下養護28 d強度可達3~7 MPa,滿足一般礦山對充填料的要求.根據料漿質量分數和坍落度關系曲線,得到了該材料制備成的可泵送膏體質量分數范圍為80.5%~83.0%.通過X射線衍射和掃描電鏡分析,膠凝材料的水化產物主要為凝膠類物質、鈣礬石和方解石.Abstract: Grade Ⅰ and grade Ⅱ fly ashes were chosen to produce a cementitious material to replace traditional cement using lime and flue gas desulphurization gypsum(FGD) as stimulation agents.Whole-tailings backfilling samples were prepared with the ratio of the cementitious material to whole-tailings being 1:4 and the ratio of water to the cementitious material being 1:1.The compressive strengths of the whole-tailings backfilling samples cured under the conditions of 45±1℃ for 3d and 20±1℃ for 28d are 5.432 MPa and 3 to 7 MPa,respectively.This generally satisfies the requirement of cemented backfilling for underground mining.Besides,relationship curves between the mass fraction of slurries and the slump were obtained and the mass fraction of the pumpable paste backfilling with the cementitious material is from 80.5% to 83.0%.By the analyses of X-ray diffraction and scanning electron microscopy,hydration products of the cementitious material are mainly gel,ettringite and calcite.
-
Key words:
- cementitious materials /
- fly ash /
- tailings /
- backfilling
-

計量
- 文章訪問數: 263
- HTML全文瀏覽量: 82
- PDF下載量: 17
- 被引次數: 0