Bonding behavior of 25Cr5MoA/Q235 hot rolled clad plates
-
摘要: 將25Cr5MoA/Q235鋼板復合板坯加熱到800~1100℃,經保溫后軋制1道次,壓下量為50%~70%,制成25Cr5MoA/Q235鋼熱軋復合板試樣.用材料力學性能試驗機測試復合板試樣復合界面的剪切強度,用光學顯微鏡和掃描電鏡觀察界面的組織.結果表明:當軋制溫度在900~1000℃時,有利于25Cr5MoA/Q235鋼的復合;道次壓下量對25Cr5MoA/Q235鋼復合板界面結合強度影響非常大,道次壓下量大,有利于形成更多潔凈、活化的新生表面,并且可以細化晶粒,提高復合板的結合強度;金屬組織中晶粒的梯度變化,有利于提高雙金屬復合材料的結合強度.Abstract: 25Cr5MoA/Q235 steel clad plates were prepared with the composite slabs heated to the temperature between 800℃ and 1 100℃, held at each temperature for 30 min, rolled one pass and reduced from 50% to 70%. Their bonding shear strengths were tested by the electron universal testing machine CMT4105 and the metallographic microstructures of their interfaces were observed by optical microscope and SEM. The results show that the rolling temperature between 900℃ and 1000℃ is favorable to the bonding of the steels and pass reduction is crucial to the bonding strength. When the pass reduction becomes large, cleaner and more activated new interfaces will be obtained and the grains will The gradient metallographic changes of grains can be refined, as a result the bonding strength can be enhanced. also raise the bonding strength of the clad plates.
-
Key words:
- bimetal composite /
- Q235 steel /
- 25Cr5MoA steel /
- bonding properties /
- rolling /
- pass reduction
-

計量
- 文章訪問數: 182
- HTML全文瀏覽量: 68
- PDF下載量: 12
- 被引次數: 0