Strengthening and Toughening of Mg-PSZ Ceramics
-
摘要: 研究了兩種MgO含量PSZ陶瓷的機械性能與電鏡組織。含7.98mol%MgO的試樣,在燒結溫度下有一部分四方相,冷卻過程完全轉變為單斜相。其中出現貫穿晶粒的孿晶,與晶界接觸處出現較寬的微裂紋,對強韌化不利。Abstract: TEM morphology and mechanical properties of two Mg-PSZ ceramics were investigated. The samples of 7.98 mol % MgO was two phases, cubic and tetragonal, at the sinter temperature. The tetragonal phase was coarse and transformed totally into monoclinic one with martensitic mechanism during cooling. Inside the monoclinic particles, there were twins developing from boundary to boundary, where appeared wide microcracks with little toughening effect.
-
Key words:
- PSZ ceramic /
- toughening /
- strengthening
-

計量
- 文章訪問數: 233
- HTML全文瀏覽量: 95
- PDF下載量: 5
- 被引次數: 0