Effect of Cold Rolling Process on Basic Feature of Formablity of the 1Cr13 Stainless Steel Sheet
-
摘要: 研究了冷軋工藝參數對1Cr13不銹鋼薄板基本成型指標的影響,找出了影響其指標的重要因素:冷軋總壓下率、退火溫度。通過研究分析指出,適用于深拉成型1Cr13不銹鋼的冷軋工藝參數為:冷軋總壓下率60%,退火溫度750℃,空冷。并從金相織構等方面對其機理進行了分析。Abstract: It has been found that main factors effecting on the forming property are the total reduction of cold rolling and the annealing temperature.The results obtained shows that optimum process parameters for deep drawing lCr13 stainless steel sheet are: the total ruduction is 60%,the annealing temperature is 750℃ followed with the air-cooling, The aspect of metallurgical structure and texlure was also discussed.
-
Key words:
- total reduction /
- metallurgical structure /
- formablity /
- stainless steel
-