Experimentation of Direct Alloying with Chrome Ores
-
摘要: 根據熱力學原理分析了鉻礦直接合金化的合理性及其影響因素,并對熔渣堿度、鉻礦加入量和還原劑的影響進行了實驗研究。其結果表明,熔渣堿度控制在1.5左右,加人鉻礦后熔渣中Cr2O3含量低于30%,先用碳還原再用硅還原,可以獲得較好的冶金效果。Abstract: The reasonableness of direct alloying with chrome ores is discussed with thermodynamical analysis as well as the influencing factors, such as the burden of chrome ores, basicity of slag and reductants. The results of experiments have shown that the basicity of slag should be around 1.5 and the chrome ore burden was limited up to 30% of Cr2O3 in slag. Carbon was used as reductant first and then silicon to continue for better metallurgical effect.
-