Direct Ageing of Alloy GH169
-
摘要: 用熱變形后的直接時效(DA處理)和標準熱處理對比試驗的方法,對DA處理在GH169合金中的實際應用進行了探討。結果表明,DA處理確可提高合金的拉伸強度,并大幅度提高光滑持久壽命。但由于塑性指標的降低而導致缺口持久和周期持久壽命的降低,并使疲勞、蠕變交互作用的蠕變損傷加劇。其原因是可能DA處理過程中晶界δ相析出過少,晶界晶內強度配合不良,達不到強韌化的作用。同時指出晶粒細化,并在變形工藝中對位錯組態進行控制,使δ相以合理的數量和形態析出,才能獲得真正應用的DA GH169合金。Abstract: For the purpose on application of direct aging (DA) GH169 in production a comparison of direct ageing treatment and standard heat treatment following hot deformation is conducted. Direct ageing treatment can get higher tensile strengthes and raise smooth specimen stress rupture lives remarkably. However, both notched specimen stress rupture aud cyclic stress rupture lives decrease because of the low ductility. The creep damage during creep and fatigue interaction condition is also enhanced. The reason may be smaller amount δ precipitate distribution at grain boundaries and the grain boundary cohesive force can not perfectly match grain strength, then the strengthening and ductility improvemeat can not reach simultaneously. Grain refinement and dislocation configuration control at the hot deformation process are most important factors to control the suitable amount and distribution of δ-phase.
-
Key words:
- direct age /
- grain size /
- GH169 alloy
-

計量
- 文章訪問數: 171
- HTML全文瀏覽量: 69
- PDF下載量: 9
- 被引次數: 0